{"product_id":"ferroinstant-titanium-coloring-bath-anodizing-tank","title":"Ferroinstant Titanium Coloring Bath - Anodizing Tank","description":"\u003cdiv class=\"dr-product-desc\"\u003e\n\u003cstyle\u003e\n  .dr-product-desc{font-size:15px;line-height:1.7;color:#3a3a3a;max-width:100%;word-wrap:break-word}\n  .dr-product-desc .section-title{font-size:1.1em;font-weight:700;margin:1.75em 0 .65em;padding:8px 12px 8px 14px;border-left:4px solid #0077c8;color:#1a1a1a;line-height:1.35;background:#eef6fb}\n  .dr-product-desc .section-title:first-of-type{margin-top:0}\n  .dr-product-desc p{margin:0 0 .9em;line-height:1.7}\n  .dr-product-desc ul{margin:.25em 0 1em;padding-left:1.3em}\n  .dr-product-desc li{margin-bottom:.45em;line-height:1.65}\n  .dr-product-desc strong{font-weight:600;color:#222}\n  .dr-product-desc .key-highlight{background:linear-gradient(135deg,#f0f7ff 0%,#e8f4fc 100%);border:1px solid #b8d9f0;border-left:5px solid #0077c8;border-radius:10px;padding:20px 22px 18px;margin:1.75em 0;box-shadow:0 2px 12px rgba(0,119,200,.08)}\n  .dr-product-desc .key-highlight::before{content:\"What sets this product apart\";display:inline-block;font-size:.72em;font-weight:700;letter-spacing:.04em;text-transform:uppercase;color:#fff;background:#0077c8;padding:5px 12px;border-radius:4px;margin-bottom:12px}\n\u003c\/style\u003e\n\u003cp class=\"section-title\"\u003e\u003cstrong\u003eMulti-purpose innovative electrolysis and restoration unit\u003c\/strong\u003e\u003c\/p\u003e\n\u003cp\u003eSince the first electrolysis device developed in 2004 and patented in 2005, the technology has advanced further. The first model could clean deposits from 2000-year-old Roman coins without damaging the base metal. With the new-generation \u003cstrong\u003eAFE-1794\u003c\/strong\u003e model, a larger multifunctional “Allround” unit was designed in response to customer requests.\u003c\/p\u003e\n\u003cp class=\"section-title\"\u003e\u003cstrong\u003eWhat this modern archaeological cleaning and metal-processing unit can do\u003c\/strong\u003e\u003c\/p\u003e\n\u003cul\u003e\n\u003cli\u003e\n\u003cstrong\u003eArchaeological restoration:\u003c\/strong\u003e cleaning hardened deposits on metal finds by electrolysis.\u003c\/li\u003e\n\u003cli\u003e\n\u003cstrong\u003eGalvanization:\u003c\/strong\u003e coating metals with different metal layers.\u003c\/li\u003e\n\u003cli\u003e\n\u003cstrong\u003eAnodizing preparation:\u003c\/strong\u003e anodizing aluminum parts before coloring.\u003c\/li\u003e\n\u003cli\u003e\n\u003cstrong\u003eElectrolytic degreasing:\u003c\/strong\u003e fully chemically cleaning parts.\u003c\/li\u003e\n\u003cli\u003e\n\u003cstrong\u003eTitanium coloring:\u003c\/strong\u003e creating decorative colors on titanium surfaces.\u003c\/li\u003e\n\u003c\/ul\u003e\n\u003cp class=\"section-title\"\u003e\u003cstrong\u003eTitanium coloring and anodizing (new feature)\u003c\/strong\u003e\u003c\/p\u003e\n\u003cp\u003eThe unit is suited to aesthetic and protective coloring of titanium parts. Titanium is colored not with dye as on aluminum, but by \u003cstrong\u003elight interference\u003c\/strong\u003e.\u003c\/p\u003e\n\u003cul\u003e\n\u003cli\u003e\n\u003cstrong\u003eHow it works:\u003c\/strong\u003e The titanium part is connected to the anode (positive pole). Depending on applied voltage, a very thin transparent oxide layer forms on the metal. Layer thickness determines how light is refracted and produces vivid colors such as \u003cstrong\u003egold yellow, purple, blue, pink, or green\u003c\/strong\u003e without paint.\u003c\/li\u003e\n\u003cli\u003e\n\u003cstrong\u003ePrecise control:\u003c\/strong\u003e An adjustable joint arm and titanium wire let parts be immersed in the electrolyte bath at the desired angle for even, spot-free color.\u003c\/li\u003e\n\u003cli\u003e\n\u003cstrong\u003eDurability:\u003c\/strong\u003e Full stainless-steel construction supports long service life with the solutions used in titanium anodizing.\u003c\/li\u003e\n\u003c\/ul\u003e\n\u003cp class=\"section-title\"\u003e\u003cstrong\u003eTechnical details and application advantages\u003c\/strong\u003e\u003c\/p\u003e\n\u003cul\u003e\n\u003cli\u003e\n\u003cstrong\u003eProtective cleaning:\u003c\/strong\u003e Electrolytic cleaning does not remove base material like abrasive methods (sanding, sandblasting). Original patina and metal structure are preserved.\u003c\/li\u003e\n\u003cli\u003e\n\u003cstrong\u003eFlexible anode distance:\u003c\/strong\u003e Two large stainless-steel anodes supplied with the unit cover the object at a 1:1 ratio. Anode distance can be adjusted manually to optimize current for object size.\u003c\/li\u003e\n\u003cli\u003e\n\u003cstrong\u003ePower supply recommendation:\u003c\/strong\u003e For full performance, a laboratory power supply of at least \u003cstrong\u003eMax 100 Volt and 20 Amper\u003c\/strong\u003e with voltage and ampere displays is recommended.\u003c\/li\u003e\n\u003cli\u003e\n\u003cstrong\u003eImportant note:\u003c\/strong\u003e Before titanium coating, thoroughly degrease and clean the titanium surface.\u003c\/li\u003e\n\u003c\/ul\u003e\n\u003cp\u003e\u003cstrong\u003eCaution:\u003c\/strong\u003e This unit is not suitable for continuous long use. After 5-minute uses, rest the unit for 5 minutes.\u003c\/p\u003e\n\u003cp class=\"section-title\"\u003e\u003cstrong\u003eHow to obtain gold yellow\u003c\/strong\u003e\u003c\/p\u003e\n\u003cp\u003eOn titanium, colors change in sequence as voltage rises. To reach gold yellow:\u003c\/p\u003e\n\u003cul\u003e\n\u003cli\u003e\n\u003cstrong\u003eCleaning is essential:\u003c\/strong\u003e Wash the part thoroughly and remove grease. Even fingerprints can cause uneven color.\u003c\/li\u003e\n\u003cli\u003e\n\u003cstrong\u003eRaise gradually:\u003c\/strong\u003e Start the unit and increase voltage slowly.\u003c\/li\u003e\n\u003cli\u003e\n\u003cstrong\u003e10–25 Volt:\u003c\/strong\u003e brown and purple tones.\u003c\/li\u003e\n\u003cli\u003e\n\u003cstrong\u003e30–35 Volt:\u003c\/strong\u003e dark blue begins.\u003c\/li\u003e\n\u003cli\u003e\n\u003cstrong\u003e45–55 Volt:\u003c\/strong\u003e light blue and turquoise tones.\u003c\/li\u003e\n\u003cli\u003e\n\u003cstrong\u003e60–75 Volt:\u003c\/strong\u003e the \u003cstrong\u003egold yellow\u003c\/strong\u003e range.\u003c\/li\u003e\n\u003cli\u003e\n\u003cstrong\u003eObserve:\u003c\/strong\u003e Immerse the part and bring voltage near 60V. When the yellow tone you want appears (from light yellow toward deep gold), remove the part immediately and rinse in pure water.\u003c\/li\u003e\n\u003c\/ul\u003e\n\u003c\/div\u003e","brand":"Ferroinstant","offers":[{"title":"Default Title","offer_id":46035159253036,"sku":"FE.5-003","price":199.0,"currency_code":"USD","in_stock":true}],"thumbnail_url":"\/\/cdn.shopify.com\/s\/files\/1\/2699\/7450\/files\/2994.jpg?v=1787583186","url":"https:\/\/www.dentrealstore.com\/en-de\/products\/ferroinstant-titanium-coloring-bath-anodizing-tank","provider":"DentrealStore","version":"1.0","type":"link"}